Are car body parts also galvanized the same way ??
ОтветитьIn this process material direct dip in dichromate tank need quenching tank .
Ответитьo beam
ОтветитьО боже. Нарушение, всех техник безопасностей в мире. Аааааааа. Ужас
ОтветитьWhy would you skip over the ACTUAL DIPPING part?
ОтветитьWhat makes it stick? And can you dip things in tin? I wish it would stay that shiny. And what makes The crystals big or small?
ОтветитьPeople gotta stop using auto focus. A camera just can’t know for sure what you’re trying to look at all the time. You twist that lens, you’re all good.
ОтветитьAmazed at all the different variations on comments of the way it’s done.
ОтветитьThat is not actual dipping.
Ответить❤️❤️❤️❤️
ОтветитьThx
ОтветитьSo why is welding galvanized so dangerous? I thought theyd be wearing respirators and such!
Ответитьthe sound is not good I am quite disappointed
Ответитьwhat percentage of metals lik zinc, aluminium and lead does bath contains?
ОтветитьThis is the best quality I’ve seen
ОтветитьThis was for school 😂
ОтветитьWhat is the maximum coating in microns that can be achieved on steel tubes as thick as 3 mm ?
ОтветитьThe bar that holds the parts is rusty.... ironic..
ОтветитьNot a respirator in sight. RIP workers
ОтветитьAntonmursid🙏🙏🙏🙏🙏🇲🇨🇲🇨🇲🇨🇲🇨🇲🇨
Ответитьthe issue with galvanizing is it makes the metal rust faster
ОтветитьJust dip my whole car and that stuff
ОтветитьGood work
ОтветитьI work maintenance in a galvanizing factory its a really cool process.
ОтветитьMy job expires 6 yes
Ответитьgood system
ОтветитьDamn you lads are some kings. I only electroplate zinc, and the 200 degree dryers i work next to make me sweat bullets enough. big ups
ОтветитьIs it a type of thermal spray coating?
ОтветитьQuestion, are zinc fumes created in the process? I work in a galvanizing facility and was wondering if breathing protection should be used around the pot.
Ответитьworkers NEED to wear gloves...overall its SAFETY nightmare...the fumes etc
ОтветитьHi,
Looking help from experienced people in Hot galvanise
We have started Hot Galvanise process in San Luis Potosi, Mexico and are having many troubles in getting the perfect final product. sometimes either zinc is getting burnt or sometimes the finishing is not coming properly. We know that we are missing many things to make it work.
Is any there anyone who could help us with this? Help will be much appreciated!
Mash Allah
ОтветитьGayet başarılı ve farklı bir tarz 👏👏👏
ОтветитьWhat is the one thing keeping the entire industry from switching to Zn-Mg-Al ternary baths? The galvanic protection offered by those are up to a few hundred times greater than normal hot dip Zn.
Ответитьola sou brasileiro e zincador profissional com a estrutura certa vocês podem dobra a produtividade
ОтветитьKaj hobe. gass catar, welider
Ответитьyou'd think they might spare a bit on their own equipment
ОтветитьQual contato de vcs
ОтветитьBrothers give me location
Ответитьbest video!
Ответитьnice!
ОтветитьThis is what we use for
Our push piers for my company. This steel is used to
Ships!
Acier galvanisé 🤙
ОтветитьSo this is where little John gets it all from
ОтветитьLil John would be living on the streets without this!
ОтветитьNow we just need an exo-friendly wood veneer tutorial
ОтветитьBeen doin this for 15yrs💪😎😎
ОтветитьI want information in this area, please
ОтветитьIts ver nice and clear explanation thankyou very much . Janardhanreddy